Electronics Forum: viewing (Page 1702 of 7892)

Multitroniks Ragen 3600 semi-auto insertion problems

Electronics Forum | Fri Apr 25 10:37:15 EDT 2003 | jonfox

I'm a former Multi field engineer and one of the last ones to work on the Ragens. Contact me offline at jonf@scc-inc.com

Electrovert Omniflow 10 Specs.

Electronics Forum | Thu Apr 24 12:45:41 EDT 2003 | cyber_wolf

Can someone possibly post a link, or get me the specs/requirements of an Omniflow 10 reflow oven ? Air consumption, power consumption, dimensions etc... Thanks

Electrovert Omniflow 10 Specs.

Electronics Forum | Thu Apr 24 16:12:47 EDT 2003 | jgregory

SrTech, contact me offline: jason.gregory@labarge.com We have two and I can get you what you need. Jason Gregory

Electrovert Omniflow 10 Specs.

Electronics Forum | Thu Apr 24 16:34:18 EDT 2003 | pjc

OmniFlo 10 Engineering Data Sheet has been sent to your SMTnet mail box. Its a PDF 818Kb.

MVT Paste Inspection GS1 machine

Electronics Forum | Thu Apr 24 13:34:58 EDT 2003 | jbservices

Can anybody point me to a web site or help with specs for MVT paste inspection GS1 machine. thanks

Black Pad

Electronics Forum | Fri Apr 25 08:09:13 EDT 2003 | razor

Thanks for response. I do wish to qualify that I got the alleged role of Nickel use for corrosion resistance from an article authored by Jason Gjesvold, IS IT REALLY BLACK PAD?, "Phosphorus rich Ni alloys are often used for corrosion resistance duri

Search Is Blanked

Electronics Forum | Tue Apr 29 11:09:21 EDT 2003 | bdoyle

Ok I fixed a couple of things in the search and now I get 7387 results for solder. I'm going to fix the "only searching in the forum" part next.

Tombstone defect

Electronics Forum | Fri Apr 25 08:48:25 EDT 2003 | davef

If what you say is accurate, two thing come to mind: * Pads on the board are incorrect for the tombstoning components. * Profile is different on the individual pads of tombstoning components. We have heard of, but never seen, components [tants] that

Tombstone defect

Electronics Forum | Thu May 01 17:49:33 EDT 2003 | jym2000

Did you check board orientation into the reflow oven? (The Layout components are the same products A & B?) Regards Jesus

Tombstone defect

Electronics Forum | Mon May 05 02:37:11 EDT 2003 | gaoliangcheng

Maybe you can check the thickness of the solder mask between the pads. If the highest of the solder mask exceed the pad,then the component which was placed will be unbalanced.


viewing searches for Companies, Equipment, Machines, Suppliers & Information

Selective soldering solutions with Jade soldering machine

World's Best Reflow Oven Customizable for Unique Applications
Electronics Equipment Consignment

High Precision Fluid Dispensers
Thermal Interface Material Dispensing

High Throughput Reflow Oven
Hot selling SMT spare parts and professional SMT machine solutions

"回流焊炉"