Electronics Forum | Thu Apr 21 12:35:15 EDT 2005 | jdumont
Well that doesnt sound very promising. What im going to do is make sure these two boards I just coated (with the RTV already cured) will be used in house only. In the future we will do any conformal coating operations before potting with whatever mat
Electronics Forum | Fri Jun 03 14:31:33 EDT 2005 | Peter
I am working on an application requiring removing BGAs from a board coated with parylene. These BGAs have low standoff with less than 0.015" after SMT soldering. Can some comment on a reliable and consistent process to perform such rework? given tha
Electronics Forum | Thu Dec 10 15:33:55 EST 2009 | duso02
We use one quite often. Our machine is a Uvitron Conveyor 40 as we are a large coating house and this allows us to process many boards. Dymax also maufactures and sells machines as well. Humiseal and Dymax both manufacture UV coatings. Emerson Cuming
Electronics Forum | Thu Apr 28 11:14:27 EDT 2005 | bbarr
If you apply the RTV after coating, what happens to bond strength since you are now bonding to the coating and not the board? Will the caps still survive vibration and shock? I specify applying RTV before coating for this reason. Am I correct? I als
Electronics Forum | Tue Feb 29 23:21:02 EST 2000 | Doug Clement
Can anyone recommend a system for conformal coating a board? We are a interested in an inline system behind our Pick-and-Place machines. Thanks Doug
Electronics Forum | Tue Feb 29 23:21:02 EST 2000 | Doug Clement
Can anyone recommend a system for conformal coating a board? We are a interested in an inline system behind our Pick-and-Place machines. Thanks Doug
Electronics Forum | Tue Aug 11 15:13:05 EDT 1998 | Xingsheng
Hi, can you please tell me how to make green coating and through-hole plating of PCB? Thanks! Xingsheng
Electronics Forum | Thu Sep 08 11:34:24 EDT 2005 | prod eng
I wonder if anybody could spec a conformal coating or simalar application, to protect PCB's at 90% humidity. Standard HPA from electrolube does not work if the humidity is in excess of 75%. Cheers
Electronics Forum | Mon Dec 21 11:31:19 EST 2009 | lynn_norman
Fusion makes UV ovens. Most conformal coating suppliers have a UV line. Great for quick cures, but the ovens interfered with our automated guided vehicles, so we had to abandon the UV.
Electronics Forum | Tue Mar 01 15:07:00 EST 2011 | dennisfo
Update on 1B73 bubbles, Changed over to a mixture of Humiseal 73 thinner with coating (25 sec on Zahn 2) observed a reduction in bubble formation (approx. 20%) but still present.