PbF PCB finish

Electronics Forum | Thu Jan 25 04:55:08 EST 2007 | greg york

Strange as we have had huge problems with Silver in Many different Assembly houses. Mainly with Nitric Acid based Silvers causing blow holes, non wetting and even the Nitric etching away the tracks on fine boards. It has been one of the main problem

Solderality problems with SN100C Lead Free Hasl

Electronics Forum | Fri Sep 22 09:45:26 EDT 2006 | bradlanger

Greg, All the above. It looked like it was going to be a drop for SNPB HASL at first but after a few thousand boards we started running into all the problems you are describing. We first started seeing non wetting on SMT pads. The solder would wet t

Lead free Solder Paste troubles !!!!

Electronics Forum | Thu Sep 23 23:42:52 EDT 2004 | KEN

The LF pastes will have virtually NO wetting spread. This is normal. LF mobilities are virtually non-existant with SAC alloys. However, the addition of varrying amounts of silver can (and does) improve mobility but, this comes with a price (paste

Solder Spotting on Gold

Electronics Forum | Thu Aug 06 09:51:20 EDT 1998 | Bob Willis

This text may be of interest to any one with tin lead spots Guide to Solder Spots - A New Plague in Manufacture ? So what are solder spots ? They appear to be the next big problem in modern reflow assembly in fact in any process that involves solder


non wetting onimmersion silver searches for Companies, Equipment, Machines, Suppliers & Information

thru hole soldering and selective soldering needs

Training online, at your facility, or at one of our worldwide training centers"
Global manufacturing solutions provider

Easily dispense fine pitch components with ±25µm positioning accuracy.
Selective soldering solutions with Jade soldering machine

Have you found a solution to REDUCE DISPENSE REWORK? Your answer is here.
Shenzhen Honreal for all your SMT Equipment needs

Nozzles, Feeders, Spare Parts - Siemens, Fuji, Juki, Yamaha, etc...