Electronics Forum | Wed Nov 25 15:16:04 EST 2009 | sforman1
Why in heavens name are you using a heat or air cure conformal coating. Why aren't you using a 100% solids UV cure system. You would never have an issue like this Sam Forman MicroCoat Technologies
Electronics Forum | Mon Sep 29 07:10:37 EDT 2008 | g2garyg2
PROMATION builds edge carry style UV systems, integrating DYMAX, FUSION and other technologies. (262) 857-3100 x 111 or www.pro-mation-inc.com
Electronics Forum | Tue Jun 04 19:33:16 EDT 2002 | rob_thomas
Dave's estimation is pretty conservative but there is a lot of equipment out there and a lot of people happy to make a sale.Implementing both mentioned processes it's difficult and time consuming .Even if you get good training from whoever sells you
Electronics Forum | Mon Mar 21 09:33:25 EST 2005 | davef
RoHS Substance||RoHS MCV Limits||Typical Testing Approaches Lead||1000 ppm* ||Wet chemical digestion followed by ICP (Inductively coupled plasma) or AAS (atomic absorption) spectroscopy ||||XRF (X-ray fluorescence) spectroscopy Cadmium||100 ppm ||Wet
Electronics Forum | Sat Sep 24 16:06:13 EDT 2011 | tech1
Okay so you are picking from a Wafer Frame and it is a UV cured tape. Who's die sorting machine are you using? You mention the ejector needles, but have you checked them? What size are the die and how thick are they? Have you checked the UV cure, i
Electronics Forum | Tue Feb 08 12:36:28 EST 2000 | Charlie
I'm looking for information from both those who do cure glue and reflow past with the same profile and those who have tried and decided against it. What were the problem? What are the limitations?
Electronics Forum | Wed Jan 03 15:11:09 EST 2007 | kennyg
Is it acceptable to apply an acrylic conformal coat, cure and then apply a silicone RTV on top (for staking tall components)? Should there be a concern with the bond between the acrylic and the RTV?
Electronics Forum | Fri Mar 14 11:18:29 EDT 2008 | operator
The way it works is the liquid solder immediatley cures (or should I say burns) the WSOL where ever it touches it. This hardens and keeps it in place and protects whatever is under it. Some of the WSOL falls of in the pot. I am suprised that the burn
Electronics Forum | Fri Mar 19 10:27:42 EDT 2010 | karlo
No clean pastes leave more flux residues. These can result in void formation and inhibtion of underfill curing. Selection of an underfill that is compatible with the flux residue is important. One company that has written about the effect of flux
Electronics Forum | Wed Jan 03 21:20:22 EST 2007 | davef
Comments are: * General purpose RTV (RTV-108) releases an acetic acid (vinegar) during cure and corrodes copper, brass and sensitive metals. It is therefore NOT for use in delicate electrical or electronic applications. However, there is an electrica