Electronics Forum | Thu Feb 23 23:27:03 EST 2006 | KEN
I thought durastone was not ESD safe?
Electronics Forum | Thu Feb 23 05:33:55 EST 2006 | teilo
Hi John We manufacture titanium component parts for wave solder machines inc retrofit kits for the conversion to lead free at a fraction of the manufacturers cost. For a quote email me at office@teiloengineering.com
Electronics Forum | Thu Feb 23 10:19:29 EST 2006 | Hiram
Hi John, I have used some wave fixtures with titanium inserts. I ordered from Pentagon EMS (503)924-2747... Turnaround time and quality are excellent. Regards, Hiram
Electronics Forum | Thu Feb 23 04:04:46 EST 2006 | Rob
We used durastone, with a profile routed out to expose certain areas & protect others. Durastone costs peanuts, and the tool room uses a small cheap Micromat router.
Electronics Forum | Thu Feb 23 05:36:09 EST 2006 | teilo
Hi Rob Can you please tell me where you can get durastone for peanuts as I find it quite expensive.
Electronics Forum | Thu Feb 23 16:08:36 EST 2006 | MARK
Hello John, I have not received the data from you. Please forward to this E-Mail MBeesley@optonline.net Best Regards, Mark
Electronics Forum | Fri Feb 24 04:36:30 EST 2006 | rlackey
Hi Ken, There may be different composites of Durastone, but there are certainly mixes out there that are. http://www.ascenteceng.com/resources/materials.html We used durastone as a carrier for flex circuits as well. Cheers, Rob.
Electronics Forum | Tue May 16 22:30:19 EDT 2006 | davef
Check the fine SMTnet Archives. For instance: http://www.smtnet.com/forums/Index.cfm?CFApp=1&Message_ID=5386
Electronics Forum | Wed Feb 22 16:42:47 EST 2006 | Mark Beesley
Hello John, There are some coatings for aluminum to eliminate solder drag out. The do not work with all fluxes it is called hardcoat anodized it is black or geen in color. Unless you have faily high volumn the hard coat cost can be as high as titan
Electronics Forum | Tue May 16 15:30:07 EDT 2006 | George
Hi John, Are you talking about cleaning the pallets after running to store them? or during production? well in any case...I recently started to use this cleaning solution "Cybersolv" from Kyzen. It is water soluble and also can be used instead of IP