Electronics Forum: shelf life (Page 29 of 38)

Losing parts in wave

Electronics Forum | Tue Oct 05 18:07:53 EDT 1999 | Bill Haynes

I hope that someone can help me with my problem! I am experiencing a lot of glued on parts falling off in the wave solder machine. A little information about my process: 1)We use Loctite 3609 glue that is used up long before its shelf life 2)Our pa

Re: Electroless Tin Plating

Electronics Forum | Sat Aug 21 12:13:17 EDT 1999 | Brian

| I am being asked, by my vendor and Purchasing people about converting from Tin/lead pads on P.C.B's to Electroless Tin Plating. | Can any one tell me what I have to change in my SMT | process (paste, reflow, etc) If any? | I ran one P.C.Boar

Re: HASL - again?

Electronics Forum | Fri Jun 18 12:20:16 EDT 1999 | John Thorup

| Now don't everyone jump on this at once, but it seems time for me to send out copies of my not even close to being dated copy of an article about HASL. Though it was published in 1992, in Printed Circuit Fabrication Magazine, and it got rave review

Re: Controlled TempHumidity rooms

Electronics Forum | Wed Dec 09 14:36:26 EST 1998 | Earl Moon

| Hi, I know for sure that by controlling temp. and humidity | conditions in SMT assy lines room, one gets advantage in | screen printing, adhesive dispensing, and pick&place | machines mainteinance. Does any one have any advice on why | else is a c

Re: Voids and BGA

Electronics Forum | Sun Mar 01 15:52:13 EST 1998 | Earl Moon

| From several months I am investigation about the VOIDS PERSENCE and his important as reliability. | One question now is : | It is possible that on the BGA components the voids are already present into the balls, before the mounting on the pcb ? | I

Re: Solder Paste

Electronics Forum | Fri Feb 20 14:33:47 EST 1998 | Dave McFadyen

Looks like (so far) we have a concensus. Follow the paste manufacturers guidelines on storage. Normally, refrigeration is required to achieve max shelf life between 3 and 6 months in original closed container. Water-wash pastes are much more active t

Adhesives

Electronics Forum | Wed Jan 09 11:09:53 EST 2002 | slthomas

Is anyone still using Loctite 348 chipbonder for bottom side attachment? Is it truly adequate for dispensing up to 18k/hour? We will be dispensing with a Camelot 2800, so somewhere in the neighborhood of 15k/hr. is as fast as we'll ever see. I'm c

Cleaning of Entek Boards

Electronics Forum | Thu Jul 18 21:04:06 EDT 2002 | davef

So, why can't you clean misprints on Entek boards? Entek: Cheap, flat, OK shelf life, not without process and fabrication issues. Your Entek organic solderability protection is probably Entek Plus [CU106A] made by Ethone OMI. Consider getting a co

HIC turn Pink for PCB-URGENT

Electronics Forum | Tue Jul 06 16:59:36 EDT 2004 | davef

I'm sorry for not being clear. The "1 thou" refers to the thickness of copper that rides below your ENIG. If your HIC card is blue that's good. If it's some other color that makes you nervous, then you make of it what you will. They're pretty muc

Warming up solder paste at start of days production

Electronics Forum | Mon Jul 26 06:32:58 EDT 2004 | cyber_wolf

Grant, The only thing that you really gain from refrigeration is a couple more months� shelf life. Refrigeration also seems to slow down flux separation. I am not sure how your paste consumption is, but we use ours up way before the expiration date


shelf life searches for Companies, Equipment, Machines, Suppliers & Information