Electronics Forum | Wed Feb 11 12:00:13 EST 2004 | Ventrista
Bad experience here too. You can do better than this for wave and reflow
Electronics Forum | Wed Feb 11 12:28:44 EST 2004 | patrickbruneel
Thanks a lot for the info. This is what I have been waiting for. Thanks again Patrick
Electronics Forum | Thu Feb 12 11:35:17 EST 2004 | Kris
what is the composition of the paste and ball ? Interesting to know why the customer is asking you to look for it Thx
Electronics Forum | Fri Feb 13 11:19:07 EST 2004 | Evtimov
Hi Bryan The answer is in the paste compozition. Balls of the BGA are usually made by eutetic solder paste.
Electronics Forum | Sat Feb 21 21:25:59 EST 2004 | Ken
Check out Technomatix Unicam quality system. Uses bar code and computer terminal.
Electronics Forum | Wed Feb 25 21:26:38 EST 2004 | davef
Start here: http://www.qualitydigest.com/pdfs/0104QD-SPC.pdf
Electronics Forum | Fri Feb 13 09:46:51 EST 2004 | roertner
You might want to check int using a BGA underfill material prior to coating.
Electronics Forum | Thu Feb 12 17:20:11 EST 2004 | adlsmt
Anyone have a flux that is good at preventing bridges for this application?
Electronics Forum | Tue Feb 24 18:04:22 EST 2004 | adlsmt
Im using Hi-Grade 1075 now. Is the 3541 a no-clean?
Electronics Forum | Wed Feb 25 08:42:23 EST 2004 | patrickbruneel
Give this one a try http://www.interfluxusa.com/Datasheets/IF2005M.html