Electronics Forum | Mon Jun 25 20:39:08 EDT 2001 | ianchan
Hi mate, no complete info given from what i see, so just some humble comments, mayhaps you review : 1) PCB pad finishing - Copper+nickle plated? coz if so, nickle is a KILLER to good solder wetting. what we did back here, was to HAL coat the nickle