Full Site - : nickel reaction to batch cleaning (Page 1 of 1)

SAC305 preforms not wetting to ENIG pad in fluxless process

Electronics Forum | Mon May 17 13:21:45 EDT 2021 | SMTA-64387881

PWB Bake out or other elevated temperture processes can cause issues with oxidation of that Nickel layer. The gold porosity can vary from batch to batch, but also process changes can contribute. Are you baking the boards or have previous reflow pro

Sm t net
Previous 1  

nickel reaction to batch cleaning searches for Companies, Equipment, Machines, Suppliers & Information