Electronics Forum | Fri Jan 10 03:40:41 EST 2020 | jakapratama
Hi, Some nano coat supplier said that you can drop water to the surface where the coating supposed to present before to check. If it's beading, it's still there. I take it that you meant by self in-house wiping of coating, yes? Stencil supplier nan
Electronics Forum | Thu Jan 09 21:12:18 EST 2020 | nizar
Hi, For the invisible nano coating, do we have any rapid method to determine nano coating worn out on stencil.
Electronics Forum | Fri Jan 10 10:37:34 EST 2020 | dontfeedphils
What sort of nano coating? The coatings that aren't snake oil tend to have a color to it. The other ones are typically wipe on and seem like a waste of time to me.
Electronics Forum | Fri Jan 10 14:49:20 EST 2020 | emeto
Steve I did investigate the transparent nano coat before for performance. We examined 3 different assemblies based in design criteria. In more simplistic designs it is not worth having it. On more challenging designs it is worth. It proved to have be
Electronics Forum | Fri Jan 10 14:41:02 EST 2020 | slthomas
I'm wondering if anyone has ever done a before/after test on the wipe-on type to see if it's any better. The factory applied stuff has been a game changer for us and as already stated, has the added benefit of a dye to indicate that it's still ther
Electronics Forum | Mon May 01 17:12:42 EDT 2000 | Joe
I have the same equipment and the same chemicals and have had the same problem. The part of the stencil which is glued to the mesh is being destroyed by the ultra sonics in the equipment. The only solution I found is to seal the glued part of the ste
Electronics Forum | Fri Apr 29 15:14:52 EDT 2022 | glasscake
second the kapton tape. Another tape we use alot of is powder coat tape (a tan color) because it has excellent heat resistance and a good adhesive that does not leave residue.
Electronics Forum | Wed Jul 20 05:49:45 EDT 2011 | kenneth0
I think you are referring to nano coatings. Try google nano coated stencils
Electronics Forum | Thu Sep 09 18:01:07 EDT 2021 | emeto
Sr.Tech, do you evaluate the SPI data to capture any wear out of the stencils/coating?
Electronics Forum | Tue Aug 20 09:26:36 EDT 2013 | proceng1
I believe that Rain-X contains silicone and Nano-ProTek solution does not. I did speak with a field service guy for Nano-Protek and he told me the special coating test pen that they offer is just a sharpie with their logo on it. Thats how I test to