Electronics Forum | Wed Feb 09 12:31:54 EST 2005 | russ
We are not doing this right at the moment but I have done it with great success. Of cource it depends on your pad layout we have a 20 mil gap in between pads, we printed at 10 mil wide with a 5mil stencil. I will try to find the glue we used, I kno
Electronics Forum | Sat Feb 06 16:42:18 EST 2021 | sg7914
Respected all; I am currently a student at RIT and working towards my master's in Manufacturing and Mechanical System Integration with a specialization in Electronics Manufacturing. I came across an interesting topic regarding the tooling and fixt
Electronics Forum | Mon Apr 25 22:56:44 EDT 2005 | davef
rush316 First, no one stated that PBB and/or PCBE are in FR4. FR4 contain tetra-bromo-bisphenol A [TBBA]. Second, there are classes [and grades] of dielectric materials used in fabricating printed circuit boards. Grades, NEMA LI-1. From these gr
Electronics Forum | Fri Jun 23 10:10:15 EDT 2006 | Gman
Some amount of voiding was always seen on sites where solder paste is printed. These voids are much smaller. However the site where a flip chip is flux dipped has never had problems with voiding. Macro voids (and huge ones at that)across the board s
Electronics Forum | Tue Aug 22 20:32:40 EDT 2006 | davef
Fixed position (mounted) [In-line] laser bar code scanners: * microscan 800.762.1149 info@microscan.com [Ken SMTnet] * symbol technologies symbol.com [Russ SMTnet] * Keyence and RVSI inline scanners [B Norman SMTnet] * Datalogic TC1100 bartec-systems
Electronics Forum | Tue Nov 11 16:30:08 EST 2008 | naynayno
Occasionally solder mask thickness is believed to be the cause of gasketing challenges during paste printing. We currently specific IPC-SM-840 on our fab drawings but this provides no limits or guidelines on thickness. I do not want to cause an unr
Electronics Forum | Tue Jul 09 15:20:19 EDT 2002 | pjc
When you look at the capabilities of Combo machines they tend to sacrifice performance when compared to separate X-ray and AOI machines, meaning they don't do either the X-ray or AOI operations as well as a machine that was designed to do only one. A
Electronics Forum | Tue Nov 11 17:35:08 EST 2008 | davef
SM-840, is a material qualification document only, with all the test requirements applicable only to a defined test coupon, not to production boards. So, it's useless for what you're trying to accomplish. As assemblers use A-610 - Acceptability Of E
Electronics Forum | Sun Mar 01 15:52:13 EST 1998 | Earl Moon
| From several months I am investigation about the VOIDS PERSENCE and his important as reliability. | One question now is : | It is possible that on the BGA components the voids are already present into the balls, before the mounting on the pcb ? | I
Electronics Forum | Wed Mar 02 18:46:02 EST 2005 | Austinj
The tendancy always has been "when in doubt, touch it up"... this is not the way to "verify the process" and is not the best strategy for multiple reasons (unessecary rework, additional labor costs, as well as making the solder joint more brittle, [i