Electronics Forum | Wed Mar 01 10:46:26 EST 2000 | Robert Hartmann
Kelvin, Thanks for the help. The actual opening size is .440 mm, but I think what you said makes sense. After discussing with the customer, it looks like it is the height which matters, more than the diameter. We have learned that the height of t
Electronics Forum | Wed Mar 01 16:59:44 EST 2000 | Dave F
Robert: Expect a 0.033" raw ball to be within 0.022" of the pad, after reflow. To be clear, that�s not a matter of shrinking by 33%. The volume of solder on the pad is the same as the volume of solder in the raw ball. It�s just that the solder is
Electronics Forum | Wed Mar 01 10:46:26 EST 2000 | Robert Hartmann
Kelvin, Thanks for the help. The actual opening size is .440 mm, but I think what you said makes sense. After discussing with the customer, it looks like it is the height which matters, more than the diameter. We have learned that the height of t
Electronics Forum | Wed Mar 01 16:59:44 EST 2000 | Dave F
Robert: Expect a 0.033" raw ball to be within 0.022" of the pad, after reflow. To be clear, that�s not a matter of shrinking by 33%. The volume of solder on the pad is the same as the volume of solder in the raw ball. It�s just that the solder is
Electronics Forum | Wed Mar 01 16:58:03 EST 2000 | Dave F
Robert: On your balls: Solder suppliers make several "standard balls" and can advise you. On your cleaner: Recycling water / direct to drain? Most batch cleaner suppliers can advise you on recycling and filtering systems to keep you out of troub
Electronics Forum | Wed Mar 01 16:58:03 EST 2000 | Dave F
Robert: On your balls: Solder suppliers make several "standard balls" and can advise you. On your cleaner: Recycling water / direct to drain? Most batch cleaner suppliers can advise you on recycling and filtering systems to keep you out of troub
Electronics Forum | Tue Feb 29 21:53:46 EST 2000 | Kelvin Chow
Dear Robert, On PBGA assembly, BGA sphere shrinkage number depends to the following factors, a. BGA Sphere size (before reflow) b. Solder mask opening diameter As far as I know, no formular has been established yet. Most of my friends just collect
Electronics Forum | Tue Feb 29 21:53:46 EST 2000 | Kelvin Chow
Dear Robert, On PBGA assembly, BGA sphere shrinkage number depends to the following factors, a. BGA Sphere size (before reflow) b. Solder mask opening diameter As far as I know, no formular has been established yet. Most of my friends just collect
Electronics Forum | Mon Feb 07 13:22:23 EST 2000 | Dave F
Brian: SMTnet has a "Terms & Definitions" section in the "Library." OA Flux. Flux, Organic Acid. A water soluble flux. Good luck Dave F
Electronics Forum | Tue May 23 15:40:17 EDT 2000 | larry
We currently use both Humiseal and Conap with OA flux. The flux MUST me cleaned off the assembly before coating. I know that Humiseal has coatings that are compatiable with no cleans as long as your processes are defined properly before your coating