Electronics Forum: phosphorous (Page 4 of 5)

Re: Black spots on gold finish pads.

Electronics Forum | Tue Dec 01 07:24:44 EST 1998 | Earl Moon

| Hi folks , | Lately we are seeing a lot of rawcards with black spots on the pads - most of them have Au finish(immersion gold) . We did a lot of inspecton after wave solder and found that only (fine pitch) QFP are affected the most. Our inspection

Re: Black spots on gold finish pads.

Electronics Forum | Tue Dec 01 07:54:49 EST 1998 | kallol chakraborty

| | Hi folks , | | Lately we are seeing a lot of rawcards with black spots on the pads - most of them have Au finish(immersion gold) . We did a lot of inspecton after wave solder and found that only (fine pitch) QFP are affected the most. Our inspec

Re: Plating Processes

Electronics Forum | Fri Oct 30 01:07:34 EST 1998 | Earl Moon

| I am a recently graduated Process Engineer. I am working for a company developing and manufacturing printed circuit boards. I am looking for a web link, magazine article, book, etc which describes the processes which happen at a board house. More s

Re: Bob Willis Free Advertising and more serious issues

Electronics Forum | Fri Aug 07 07:44:56 EDT 1998 | Earl Moon

| | | No sour grapes, | | | This has gone on too long. I expect no free advertising, nor do I seek it. It is clearly understood Bob is an industry leading consultant. What is not understood, at least by me, how he is allowed to "advertise" so freely

Electroless Nickel without gold immersion

Electronics Forum | Tue Aug 20 18:15:02 EDT 2002 | davef

Haaaaa!!!! Soldering to plastic!!!! An apt analogy!!! I like to compare it to soldering to dirt. Some thing. In fact, you are soldering on nickel, when soldering on many things. It�s just that the gold, er Pd, flash enables the wetting mechanism

Re: Storage life of Gold Finish Boards

Electronics Forum | Mon Jan 18 10:01:16 EST 1999 | John W

| | | | Folk's, | | | | | | | | I'm looking for information of how long you cna store a gold finish PCB before building it. I know there are problems with the gold disappearing into the underlying nickle over time / temperature etc but exactly how l

Re: Storage life of Gold Finish Boards

Electronics Forum | Tue Jan 19 11:12:41 EST 1999 | Dave F

| | | | | Folk's, | | | | | | | | | | I'm looking for information of how long you cna store a gold finish PCB before building it. I know there are problems with the gold disappearing into the underlying nickle over time / temperature etc but exactly

Re: Black spots on gold finish pads.

Electronics Forum | Tue Dec 01 09:02:18 EST 1998 | Earl Moon

| | | Hi folks , | | | Lately we are seeing a lot of rawcards with black spots on the pads - most of them have Au finish(immersion gold) . We did a lot of inspecton after wave solder and found that only (fine pitch) QFP are affected the most. Our in

Re: Black spots on gold finish pads.

Electronics Forum | Fri Dec 04 20:26:34 EST 1998 | kallol Chakraborty

| | | | Hi folks , | | | | Lately we are seeing a lot of rawcards with black spots on the pads - most of them have Au finish(immersion gold) . We did a lot of inspecton after wave solder and found that only (fine pitch) QFP are affected the most. Ou

Re: Black spots on gold finish pads.

Electronics Forum | Fri Dec 04 20:37:45 EST 1998 | kallol chakraborty

| | | | | Hi folks , | | | | | Lately we are seeing a lot of rawcards with black spots on the pads - most of them have Au finish(immersion gold) . We did a lot of inspecton after wave solder and found that only (fine pitch) QFP are affected the most