When you say "No wetting" you mean the paste looks the same as it did going in but dried out? Or is it that you are not getting toe fillets?

Hitachy QFP 256 leads problems

Electronics Forum | Tue Mar 20 17:53:44 EDT 2007 | diesel_1t

is not getting toe fillet, you can se like a "paste dome" on the pad so the paste is not flowing to the pin...

Burr Brown ICs bad solderability

Electronics Forum | Mon Dec 01 13:17:43 EST 2008 | realchunks

Jandon, what is wrong with the picture you posted? Looks good to me? The first pix Wewilldoit posted were kinda scetchy except for the one with the bent up lead. It's not the toe fillets people - it's the heel fillets you have to look at.

Toe down configuration

Electronics Forum | Mon Jul 11 15:30:52 EDT 2011 | dmiller

Take a picture of one that just barely meets specs. Take a photo of this, either under a scope or with one of those USB scopes. Then use the photo for whatever instructions you provide to the operators.

Toe down configuration

Electronics Forum | Sun Jul 31 10:06:51 EDT 2011 | davef

Try the NASA Workmanship Standards Inspectors Pictorial Reference document: http://workmanship.nasa.gov/lib/insp/2%20books/frameset.html Look at Section 7.08 SURFACE MOUNT TECHNOLOGY (SMT) BUTT "I" LEADED PACKAGES

Fuji CP6 feeder manual request

Electronics Forum | Tue Mar 25 08:51:29 EDT 2014 | sumote

I don't want to step on Han's toes here. If he does not send them to you, then let me know and I will send you the ones he sent me.

Profiling LQFP-144 with ground plane

Electronics Forum | Thu Feb 24 20:13:22 EST 2022 | dwl

They don't look that bad, especially for SN100. There is evidence of wetting on the toe and the paste on the pad seems to have reflowed properly. What does the heal look like? That's the more critical part of the solder joint for Gull leaded parts.

Re: footprint formula

Electronics Forum | Wed Mar 08 10:52:27 EST 2000 | Wolfgang Busko

Hi Jacqueline, for the "manufacturing allowance" IPC says FAB.TOL. is the board manufacturing tolerance and PLACE ACRCY is the pick and place accuracy. For 0,8 mm pitch they give for both values 0,1 mm. Solder joint design goal data comes from empir

Re: footprint formula

Electronics Forum | Wed Mar 08 10:52:27 EST 2000 | Wolfgang Busko

Hi Jacqueline, for the "manufacturing allowance" IPC says FAB.TOL. is the board manufacturing tolerance and PLACE ACRCY is the pick and place accuracy. For 0,8 mm pitch they give for both values 0,1 mm. Solder joint design goal data comes from empir

1206 Cap on 0805 Pad/Land

Electronics Forum | Thu Jan 24 04:54:43 EST 2002 | wbu

Well Greg, I don�t know YOUR 0805 Pads but if you look at the recommended pattern for 0805 in IPC-SM-782 you might notice that the Z-dimension is somewhat about the size of your 1206 part length. With that and assuming that you ask if the results wi


toes searches for Companies, Equipment, Machines, Suppliers & Information

Circuit Board, PCB Assembly & electronics manufacturing service provider

Nozzles, Feeders, Spare Parts - Siemens, Fuji, Juki, Yamaha, etc...
used smt parts china

High Throughput Reflow Oven
SMT feeders

Training online, at your facility, or at one of our worldwide training centers"
Hot selling SMT spare parts and professional SMT machine solutions

500+ original new CF081CR CN081CR FEEDER in stock