Electronics Forum: pcb finish (Page 45 of 78)

Wave Soldering Ceramic PCB's

Electronics Forum | Thu Aug 09 16:41:12 EDT 2001 | johnw

Dave , you know it's your cheery disposoition I love.... Ok so the process: Process is Double sided reflow for SMT & PTH via the wave. Like I said or did I, I forget and can't check back...it's a spray fluxer with noclean mutlicore NR3s-06 water b

Immersion white tin wave soldering problem

Electronics Forum | Fri Dec 16 03:47:46 EST 2005 | gpaelmo

Anyone have problems wave soldering white tin finish? We are an ems and our customer provides us the pcb's. SMT and TH components on the board. SMT is fine but when we wave solder, wetting to top side is very poor (solder only flows half way up). We

Bare PCB Fabricators

Electronics Forum | Thu Jul 20 10:34:15 EDT 2006 | Bill Csonka

John. My name is Bill Csonka. I am an x pcb designer now sales engineer representing Photocircuits Inc. out of Glen Cove, New York. Photocircuits is the first and oldest domestic PCB supplier in the USA originally founded in 1950. Traditionally, the

Immersion Gold over Nickle de-wetting problem

Electronics Forum | Fri Mar 07 10:51:58 EST 2003 | MA/NY DDave

Hi O'Conner, I hope you also tell us what Universal-GeorgeW discusses with you. It is a little strange seeing his name on this list and his phone number. Gee I can give you his email address but won't.. Again distance engineering is tough. I woul

Solder in via holes causing printing problems

Electronics Forum | Thu Jan 06 06:15:49 EST 2005 | mattkehoe

We need some opinions about a situation that is causing problems in our process. The pcb's in question are .125 thick with a HASL finish. The boards are coming in with a large amount of solder trapped inside the via holes. Sometimes this solder is ac

Regarding the choosing of right Suface Finishing

Electronics Forum | Mon Apr 27 11:20:18 EDT 2015 | anirudh_thabjul

hi everyone, I want to prototype my PCB. i have designed entire thing and also created GERBER files. Now i want to be prototyped. So, While searching online PCB manufacturing Companies, I found Many companies. But everywhere it is mentioned choose

Re: Detecting lifted leads on QFPs

Electronics Forum | Fri May 28 16:30:39 EDT 1999 | JohnW

| Yes l know this problem keeps cropping up on the forum but l've missed some of the follow-ups. | | Our problem is that the lifting only occurs on 3% of production so actually detecting an improvement is difficult. We're actually having to inspect

Re: silver finishes on pcbs

Electronics Forum | Wed Dec 13 20:30:59 EST 2000 | Dave F

Immersion Silver PCB Surface Plating - Dennis VanBuren 14:21:24 02/01/2000 [Wudja mean "not much luck" searching the archives? What is this haggis???][Is that like saying "what is this chopped liver??"]

should gold pads be pretinned, what issues are known are there?

Electronics Forum | Wed Sep 18 18:10:15 EDT 2002 | davef

IMHO, this finish is more cosmetically appealing than technically desirable (and VERY profitable for the PCB maker). That editorial comment aside, you're correct. Increasing the concentration of gold: * Hardens the solder. * Increases the liquidou

HIC turn Pink for PCB-URGENT

Electronics Forum | Tue Jul 06 08:04:01 EDT 2004 | ANDREW

Thanks Dave, The surface finish is ENIG.Is it ok not to bake even though the HIC has changed color? What is the shelf life for ENIG boards?


pcb finish searches for Companies, Equipment, Machines, Suppliers & Information

Precision PCB Services, Inc
Precision PCB Services, Inc

Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.

Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider

1750 Mitchell Ave.
Oroville, CA USA

Phone: (888) 406-2830