Electronics Forum | Mon Sep 14 20:19:33 EDT 2020 | kumarb
Hi. 1) recommend to phone up Heller for assistance on this case 2) using the wakeup profile, can you confirm if the problem remains or not when you skip the warm up of zone # 2? 3) each zone is based on 2 heaters (this is what we have on our 1809e
Electronics Forum | Thu Apr 29 17:52:33 EDT 2021 | mike_infl
We have an assembly which we are trying to machine pick and place a Mil-Max pin that is .020 dia placed in a .026 hole. The board is .1125 thick. We have to place 106 of these pins. Without going into the challenge of getting proper hole-fill to me
Electronics Forum | Tue May 18 08:37:48 EDT 2021 | jtautomation
Shenzhen JT is a leading intelligent equipment and advanced manufacturing system supplier that integrates R&D, production, sales and service. Shenzhen JT is established in July 1997,listed on 10 Oct.,2014 (Stock Code 300400),registered Capital
Electronics Forum | Fri Feb 18 13:55:12 EST 2022 | cbart
One thing to think about is keeping the machine running! the biggest thing I would be looking at or into is availability of spare parts and tech support. Call the equipment manufactures and see if they are still supporting the machines, both with tec
Electronics Forum | Mon Jul 31 12:04:42 EDT 2023 | spoiltforchoice
You could spend 30 mins inspecting a modestly complex board manually using a magnifier/scope and still miss things. Humans get distracted, bored and tired. It is also difficult or impossible to visually inspect some faults like mild tombstones or qu
Electronics Forum | Fri Jan 05 17:25:30 EST 2024 | ankitgun
My company recently acquired the Vitrox-V510 Optical Inspection Station, equipped with the 'V510 Series' software. However, I've noticed that the software appears to be outdated and doesn't meet modern standards. It lacks a comprehensive component li
Electronics Forum | Sun Apr 25 11:30:12 EDT 1999 | Earl Moon
| Hello all, | | Our guys here still have some questions on the "optimized" profile which sees a more moderate ramp up straight to reflow temperatures versus the conventional profile which has a plateau at around 150 Celsius. If the optimized profi
Electronics Forum | Mon Apr 06 12:32:20 EDT 1998 | Roxanne Picou
March 31, 1998-Austin, TX --- Austin American Technology announces a new Pre-Wash feature for the Mega� II to operate in conjunction with AAT's patented closed-loop regenerative cleaning process. This feature allows for an optional dual chemistry
Electronics Forum | Fri Mar 21 15:51:23 EDT 2008 | g2garyg2
Thought I would reply and try to assist. PROMATION, my company, also manufactures Diode Laser soldering systems but with this stated we also manufacturer iron tip systems, soft beam systems and hot air solutions. The reasons are simple. Diode Laser
Electronics Forum | Tue Sep 29 21:39:07 EDT 2020 | kylehunter
Hi, We are currently working on a board that has 3x 50-pin THT at 1.27mm pitch each. This is too small for us to be able to consistently do on our selective solder. We are instead considering pin in paste. The connector we are using can be spec'd at