Electronics Forum: what (Page 477 of 1843)

Matte tin finish

Electronics Forum | Wed Aug 04 16:49:24 EDT 2004 | jim_bob

Regarding Lead Free component finishes, vendors are zeroing in on matte tin plating as the finish of choice. What test are performed, to determine if a finish is "matte" type (vs. non-matte)?

Matte tin finish

Electronics Forum | Wed Aug 04 18:38:53 EDT 2004 | davef

whiskers / "matte" => no whiskers. Look here: http://nepp.nasa.gov/whisker/anecdote/20year/ There. Nice going. What a buzz killer. I've got to got find some donuts, cold pizza, er whatever.

Screw

Electronics Forum | Thu Aug 05 11:37:24 EDT 2004 | Andrew

I was told by the customer to change the screw with washer to a screw without washer as the washer causing the overlay Lexan Material underneath the washer to bulge.What should I be looking at to make this change?Can I just use the same screw without

Screw

Electronics Forum | Thu Aug 05 13:48:37 EDT 2004 | davef

We'd guess. What does your customer say? If my customer gave me a written order to do something, I'd do it, unless he was wacked.

Plating Thickness at Via Hole

Electronics Forum | Thu Aug 05 20:42:11 EDT 2004 | Andrew

If the moisture does not has path to escape,what will happen to the entrapped moisture ,will there be a problem in the asssembly process?

Questions about SMT Process Control

Electronics Forum | Mon Aug 09 11:47:52 EDT 2004 | MM

Hello, I'd like to consult somebody here about how to do the inspection of solderablity of a PWB. what is the root cause about the cold soldering in SMT.

CRACKED COMPONENTS DURING DEPANELIZATION

Electronics Forum | Tue Aug 10 15:19:09 EDT 2004 | davef

Hey Bob, turn DOWN the volume. Waint daff yano!!! On the surface of things, if you�ve been to a dozen board houses that have not been able to properly separate boards, we�d kinda be inclined to think it�s you and not them. [In your defense, we hav

soft gold vs immersion gold

Electronics Forum | Thu Aug 12 14:50:12 EDT 2004 | russ

This is interesting, I was once told by a PCB supplier that "soft gold" was immersion and the "hard gold" was the plated. But I agree with Dave F., Chris, what's going on? Russ

soft gold vs immersion gold

Electronics Forum | Mon Aug 16 16:26:19 EDT 2004 | Kris

what about areas that are soldered ? This is def not a Enig process and the specs are as they are not sure why thanks a lot for your help

Efficiency Rate...

Electronics Forum | Thu Aug 12 10:02:00 EDT 2004 | JB

There is a lot of debate over efficiency rates in our group, what percent would indicate that we have a good efficiency rate in our SMT production lines? Ours vary from 40- 60% We are constantly trying to improve this numbers, but I am curious as wer


what searches for Companies, Equipment, Machines, Suppliers & Information

Solder Paste Dispensing

Training online, at your facility, or at one of our worldwide training centers"
Thermal Interface Material Dispensing

High Resolution Fast Speed Industrial Cameras.
Pillarhouse USA for Selective Soldering Needs

Nozzles, Feeders, Spare Parts - Siemens, Fuji, Juki, Yamaha, etc...
best pcb reflow oven

High Precision Fluid Dispensers
Hot selling SMT spare parts and professional SMT machine solutions

"回流焊炉"