Electronics Forum | Wed Apr 11 11:02:53 EDT 2001 | dave
Hi I found it's hard to attach thermocouple on profile board at fine pitch component by high temp solder. Does any one know the good way to do it? Thanks in advance. Dave
Electronics Forum | Tue Jan 15 10:53:18 EST 2013 | boriskilk
We wouldn't advocate extending the soldermask beyond the component body but yes to ganging for fine pitch. To ensure we don't run into issues with flaking our preference is not to add solder mask when the space between pins is less than 6 mil.
Electronics Forum | Wed Sep 18 18:48:33 EDT 2002 | davef
Fabs can produce a solder mask web between 20 pitch leads, but I've never seen a web for 16 pitch leads. Although, I would like know a supplier that can lay-down a fine web. Minimum solder mask web width is about 0.004 thou. An absolute mininum o
Electronics Forum | Wed Sep 18 10:06:30 EDT 2002 | Bob M
I place 15-20 mil a lot. You need to look at your pad to apature reduction. Your stencil thickness. The type of paste your using. We use 2-5 mil reduction on each side as a general rule on fine pitch. This varies depending on pad width. We also use 5
Electronics Forum | Thu Sep 19 12:08:39 EDT 2002 | ccross
I would like to thank everyone for their time and replies
Electronics Forum | Thu Sep 07 08:44:17 EDT 2006 | vicknesh28
Did check the coplanarity of the failed lead and found it to be as good as the wetting leads.
Electronics Forum | Thu Sep 07 18:32:51 EDT 2006 | vicknesh28
Yes the part is reworked. It solders when it's reworked.
Electronics Forum | Fri Dec 07 02:53:26 EST 2012 | beta
no expert but would using a smaller diameter nozzle help in anyway?
Electronics Forum | Fri Dec 07 02:55:24 EST 2012 | aj
I am no expert but would using a smaller nozzle help in anyway?
Electronics Forum | Wed Dec 12 16:16:39 EST 2012 | tombstonesmt
Nitrogen at nozzle supply is at around 47.5cfh.