Electronics Forum: gold brush plating (Page 6 of 63)

gold connectors

Electronics Forum | Fri May 31 08:51:09 EDT 2002 | zanolli

Hello Dave, As related to connector mating interface, fretting corrosion is the oxidation of the contact points, causing high resistance across the interface. Fretting corrosion is caused my micromotions in the interface exposing the metalized conta

Connector leads plating

Electronics Forum | Tue Dec 10 10:26:56 EST 2002 | davef

Questions are: * What is the current plating on the connector that is over the "plating of the leads is Nickel (99.9% purity)"? * What are the temperatures and durations at those temperatures that you read on these connector leads? * What solder allo

Connector leads plating

Electronics Forum | Tue Dec 10 19:30:49 EST 2002 | Vijay

Hi Dave, The peak temp on the leads is 216-218 Deg C and duration above MP (179 degC) is 55-60 sec. Alloy(solder paste) used 62 Sn,36 Pb 2Ag (Alpha WS 609 Ty 3 Water eash) This is a SMT connector wth Gulwing leads Gold plating on the PCB is 2-5 micr

soft gold vs immersion gold

Electronics Forum | Thu Aug 12 14:50:12 EDT 2004 | russ

This is interesting, I was once told by a PCB supplier that "soft gold" was immersion and the "hard gold" was the plated. But I agree with Dave F., Chris, what's going on? Russ

Re: PWB plating

Electronics Forum | Wed Feb 03 22:47:48 EST 1999 | Chris G.

| Hi! | | Does anyone know any roadmaps for board plating materials. Especially I'm interested in finishes, which are plated onto copper. | | Teemu M�kiniemi | Teemu, For some time now, as I am sure you are aware, the PCB industry has been tryi

soft gold vs immersion gold

Electronics Forum | Wed Aug 11 18:36:03 EDT 2004 | davef

90 Knoop. Q2: Thickness is 4 to 10 u" for Au and 300 to 400 u" for nickel A2: This looks like a ENIG spec. Although, the Ni is quite heavy, 150 uin is sufficient for most applications. [IPC-4552 ENIG specification: * Gold thickness of 0.075 - 0.125

About the PCB gold finger contamination.

Electronics Forum | Thu Sep 19 17:14:02 EDT 2002 | davef

Comments are: * Use an eraser if the surface of Au is not clean, but make sure the eraser has no/low ionics (such as sulfur that is a common additive for rubber). * If the plating surface required eraser to remove the top surface, the plasma normally

solder pad with nickel plating

Electronics Forum | Wed May 11 13:27:30 EDT 2005 | Sam Ho

i want to know which type of solder paste and reflow profile can support the solder pad with nickel but not covered gold on the pcb.

tarnishing gold surfaces

Electronics Forum | Fri Nov 26 05:22:44 EST 2010 | 89jeong

Hello Esoderberg. Did you get the analyis report from your vendor? If so, could you pls share it wiht us? Based on my experiance, this issue may be caused by the Au plating. You need to ask your vendor to check the Au thickness or Au plating proces

SMT gold plated components

Electronics Forum | Thu Aug 07 09:14:02 EDT 2003 | Carol

Thanks Dave, Much appreciated. Carol


gold brush plating searches for Companies, Equipment, Machines, Suppliers & Information

Thermal Interface Material Dispensing

High Precision Fluid Dispensers
pressure curing ovens

Best Reflow Oven
SMT feeders

World's Best Reflow Oven Customizable for Unique Applications
Circuit Board, PCB Assembly & electronics manufacturing service provider

Wave Soldering 101 Training Course
Electronic Solutions R3

Thermal Transfer Materials.