Electronics Forum | Mon Feb 27 17:08:08 EST 2006 | barryg
we here are setting up our lead free process. Was curious about how others handle these issues. 1) Do you physicaly segregate leaded from non-leaded (different storage areas, shelving) for part storage? 2)Do you have a seperate board washer just for
Electronics Forum | Tue Feb 28 07:50:06 EST 2006 | amol_kane
we have used blue and red color solder mask on a trial basis for our LF assemblies. We are performing expts using Imm Sn and Imm Ag to determine the best surface finish. Also, we pass the LF baords thru the same inline wash as you dont wash away the
Electronics Forum | Tue Feb 28 06:55:44 EST 2006 | Rob
Hi I've used the following: SAP Connect & Go (or SAP in a box - designed for smaller companies)- despite the description a LOT of set up work, but not bad once you get the hang of it. Costs lots to change things though. Tetra CS3 - YUK! MFG Pro -
Electronics Forum | Fri Apr 21 23:24:06 EDT 2006 | SD
I can't tell you what's good, but I can tell you what's bad. We use JD Edwards. To give you an idea of how well it is suited to the electronics environment, most of the help screens, should you be able to find them, use recipes for bread and food
Electronics Forum | Tue Mar 07 14:41:42 EST 2006 | bman
"Would you be able to use a piped water eye wash system? That way the water is always fresh." That's what you would think, but I've heard otherwise. If you don't flush them out regularly, the water will sit in the pipes and start coroding them. If
Electronics Forum | Tue Mar 07 14:18:32 EST 2006 | James
Billy, I have to disagree with you. We inadvertently soldered a Pb BGA with SAC305 paste and then had it micro sectioned and spectrum analyzed. Imagine our surprise when we saw the spectrum analysis showed Pb. The micro sections showed none to ac
Electronics Forum | Tue Mar 07 23:50:35 EST 2006 | karenp
Thanks guys ... you gave me some ideas, I'm trying to use the camera inspection in the gemini, I use it, but i don't have a "Golden dot" as you said Pete, i'm trying with DOE analysis.. I hope can get something good, and help the team with the missin
Electronics Forum | Tue Mar 07 08:48:55 EST 2006 | samir
Our ICT Guy here at my company loves to use lots of via holes as test points - via holes which are 0.040" diameter, and spaced at 0.004" edge to edge spacing! He doesn't like to tent the via's either, so I always battle via-to-via shorts at the wave
Electronics Forum | Thu Mar 09 16:29:35 EST 2006 | russ
Will the Pb part handle 240C? That is the first question that you need to answer. If it will then yes I would run the pbfree paste and profile. I assume that all other components are pbfree. If not, the same questions will need be asked as for th
Electronics Forum | Fri Feb 16 11:37:58 EST 2007 | hectorsmtnet
I have been using the Loctite Multicore WS200 with great results for the last two years. We also use the lead free version WS300. I like the flux chemistry (which is the same for both products); it really withstands long soaking times and with very g
Buyer, Seller, Broker of Electronic Assembly Equipment
Equipment Dealer / Broker / Auctions
309 West Pickle Alley
Rushford, MN USA
Phone: 507-864-7477