Electronics Forum | Wed May 20 17:00:56 EDT 2009 | dyoungquist
We just placed a 56 pin QFN, 1 per board, on 10 boards and had zero defects. A good paste job, proper placement and a correct oven profile are the keys. If these are set up correctly, on larger runs your defects won't be zero but they should be le
Electronics Forum | Thu Aug 08 13:09:38 EDT 2013 | cyber_wolf
Hege, there is no actual calibration of the thermocouple itself. You can however verify that they read correctly. Heller sells an option on their reflow ovens specifically for this purpose. I hoping that someone chimes in here that is NADCAP certifi
Electronics Forum | Thu Jul 22 17:39:58 EDT 2021 | proceng1
We do use a company for custom fixtures, but we also make some in house. The biggest hurdle for a board that requires a fixture to go through printing and SMT is that the board has to be the tallest thing. So any hold downs or locating hardware has
Electronics Forum | Wed Sep 25 10:56:27 EDT 2002 | xrayhipp
Yeah, perhaps lean more towards a ramp-to-spike profile - reducing the soak time and add a littel heat to your temp above liquid. This has worked for us with water soluable paste as we are not required to use no-clean and utilizing a 6-zone oven. G
Electronics Forum | Wed Mar 05 03:43:58 EST 2003 | testing
Hi, Mike Thanks for the reply With your oracle system were you able to perfom SPC analysis? and if possible do you have any Material that may be helpful for me to get my system setup i.e. whether through Excel, Access, Oracle etc. + What are your
Electronics Forum | Tue Sep 23 23:19:34 EDT 2003 | RLW
If you have a board that you've run several times, now you run it and like before all settings are the same, but now you have 0603's randomly skewed or an inch or so away from their intended pad (as if popped up in the air), or an occasional 7343 cap
Electronics Forum | Fri Jul 28 14:34:13 EDT 2000 | Gary Simbulan
Belive it or not, these boards were run through a Centech batch mode Vapor Phase machine. Single stage top side IR preheat. Vapor temp 218 C. Solder paste is an SN62 RMA.The boards were FR4 8 layer w/ solder mask, fairly conventional as might be e
Electronics Forum | Fri Dec 15 18:36:46 EST 2006 | Grant
Hi, I have noticed we are getting residue on our wave pcb's and it's worse with lead free, since we changed to the flux we are using. We are currently using Avantec VOC Free flux model Ecofree 303. It looks like it's made in Malaysia. Does anyone h
Electronics Forum | Mon Apr 30 18:17:16 EDT 2001 | ianlg
Hi Barry Unable to assist on specifics but I can tell you that some 74 100is machines were built. The majority residing in China Imported in by Wong King Kong Ltd ( Johnson lee Tel 00852 2357 8888 ) Most are at either Flextronics or Roslare. You mi
Electronics Forum | Thu May 24 09:11:12 EDT 2001 | Grant Petty
Hi, I would agree. We purchased a TP9 just the slow machine, but we were a small company at the time, and it worked fantastic. Almost no maintenance, and it's a dream to changeover. The serivce in Australia is also very good, but that does not appl