Electronics Forum | Mon Jun 28 21:07:00 EDT 1999 | Deon Nungaray
| Hey there gang, how's it going ? | | Anyway's here's my probelm, got a new product to build double sided reflow, lot's of so20's and PLcc's 1206's, 0805's the usual stuff. Probelm is all the pad spacing of the 1206's are too big, my component's ar
Electronics Forum | Mon Jun 14 13:47:54 EDT 1999 | Chrys Shea
| We are a medium sized PCB assy. house manufacturing about 2000 motherboards a day. There is a major problem we are facing at the wave soldering stage, i.e. warpage of the PCB. As soon as the PCB touches the wave it warps severely from the centre
Electronics Forum | Wed Jun 16 07:34:17 EDT 1999 | Glynn Technologies and Manufacturing
| | We are a medium sized PCB assy. house manufacturing about 2000 motherboards a day. There is a major problem we are facing at the wave soldering stage, i.e. warpage of the PCB. As soon as the PCB touches the wave it warps severely from the centr
Electronics Forum | Wed May 26 10:00:03 EDT 1999 | David Scott
| | | | | | | | | | | | Any suggestions on how to maintain Adhesive dispensing nozzles??? They seem to plug up over night and it is starting to get on my nerves. We have tried leaving the nozzles in the machine, removing them and soaking in alcoh
Electronics Forum | Fri Aug 31 08:45:33 EDT 2001 | 0704494250
Hey peoples, We are working with the dairy > industry out here and they asked us to start > reworking all there boards for them. Of course we > said yes, hehe. Only we didn't know what them > farmers coated them boards with. It turned out to
Electronics Forum | Mon Apr 26 16:14:08 EDT 1999 | John W
| Hi Murray! | | Justin pretty much summed things up...covered all the points. So I'm just gonna give you my preference of what I like other than HASL finish. | | Electroless Nickle/Immersion Gold...nice flat pads...hmmmmmmm, Steve likes flat pads.
Electronics Forum | Tue Apr 27 05:04:50 EDT 1999 | Charles Stringer
| Hi Murray! | | Justin pretty much summed things up...covered all the points. So I'm just gonna give you my preference of what I like other than HASL finish. | | Electroless Nickle/Immersion Gold...nice flat pads...hmmmmmmm, Steve likes flat pads.
Electronics Forum | Sun Apr 25 11:30:12 EDT 1999 | Earl Moon
| Hello all, | | Our guys here still have some questions on the "optimized" profile which sees a more moderate ramp up straight to reflow temperatures versus the conventional profile which has a plateau at around 150 Celsius. If the optimized profi
Electronics Forum | Wed Mar 24 23:04:00 EST 1999 | Al O Owzitgon
| We are dealing with down time accredited to the Pumps getting clogged with dried glue. We have decided to purge all spindles at 6 hour intervals. We are looking at making this process automated. Has anybody tried this and if so, is there a way to s
Electronics Forum | Thu Jan 28 15:53:12 EST 1999 | Dave F
| | Hello Netters, | | | | I need some info, Earl or Dave, I have a PCB that exhibits a white layer on solder side. It does not appear to be surface residues (IPA has no effect), but looks like its under solder mask. My first guess is that the LPI