Electronics Forum | Mon Sep 05 12:11:38 EDT 2016 | sarason
The next question how do you do repair through conformal coating . Opps! Better off having done all your inspection and testing first! Hopefully your question is for service! regards sarason
Electronics Forum | Mon Jul 16 07:10:09 EDT 2012 | mccabekev
I have found that Edding do an aerospace marker, which is water based and does not run with the conformal coating. However, this washes off prior to the coating so it is not much use. Looks like we are just going to have to put some clear tape over
Electronics Forum | Tue Jul 03 10:27:57 EDT 2012 | blnorman
Check with the coating manufacturer and see if they can offer a solution.
Electronics Forum | Tue Jul 03 10:50:33 EDT 2012 | doncattoni
Try this: http://divbio.com/solventresistantpenblack.aspx
Electronics Forum | Mon Jul 23 15:37:40 EDT 2012 | rway
mccabekev, How are you applying the mark? Can you scribe the board?
Electronics Forum | Mon Sep 05 16:24:09 EDT 2016 | davef
inspect => conformal coat ... and standards are aligned with that philosophy. I can imagine doing a good job inspecting assembly after being coated with particular coating thickness, optical properties, lighting conditions. Ultra-thins are so thin
Electronics Forum | Mon Oct 14 15:13:52 EDT 2013 | esoderberg
Does anyone have a novel idea on how to protect the flex area during conformal spray coating? Currently using Humiseal T30 on the flex but it has to be removed very carefully to insure coating stays intact on the board.
Electronics Forum | Mon Jul 02 08:57:21 EDT 2012 | dontfeedphils
It'll probably help to know what type of coating you're using on your boards, how it's being applied, and how it's being cured.
Electronics Forum | Tue Jul 03 03:12:20 EDT 2012 | mccabekev
Unfortunately our customers expect this coating on the boards so that is not an option. There must be something that can mark underneath without washing off. The silk screen doesn't wash off
Electronics Forum | Tue Jul 03 03:13:14 EDT 2012 | mccabekev
Unfortunately our customers expect this coating on the boards so that is not an option. There must be something that can mark underneath without washing off. The silk screen doesn't wash off