Electronics Forum: laminates (Page 8 of 48)

Non-halogenated PCB

Electronics Forum | Wed Jul 19 11:06:42 EDT 2000 | polymer

Where can I find laminates containing non-halogenated PCB? I'm especially interested in FR-4 and CEM-3, 1.6 mm 25um. Thanks in advance! Dr. Lennart Johansson Polymer Support

Punch Force

Electronics Forum | Mon Apr 02 09:42:35 EDT 2001 | davef

Check "Chapter 5: Punching Grade Of Copper Laminates" by RJ Konsowitz in "Printed Circuits Materials Handbook" edited by MW Jawitz

BGA short at same spot after few time rework.

Electronics Forum | Wed Apr 25 23:51:13 EDT 2001 | spchua

Hi, Guy, please check the lamination of the PCB's; or the the BGA rework machine, some things like m/c levelling, and force placement head

Re: Industry Challenges

Electronics Forum | Thu Jul 20 14:25:03 EDT 2000 | Bob Willis

Better design for manufacture Better education for engineers in manufacture at college and university Realising that there is just so far you can push FR4 laminate Finding a way of making all the knowledge in our industry available to those future en

PCB Laminate Materials

Electronics Forum | Wed Jul 18 20:58:54 EDT 2001 | Charles A. Harper

Two more recent books are Electronic Packagind and Interconnection Handbook,Third Edition,2000; and High Performance Printed Circuit Boards,2000.I served as Editor for both.Charlie Harper PS to Dave Fish-Please contact me regarding two new books usef

Re: fr4 material

Electronics Forum | Wed Mar 10 18:37:27 EST 1999 | Earl Moon

| I am looking for a supplier for bare fr4 material. I use the fr4 for fixtures and my supply has run out. A supplier in the new england area would be the best. | thank you | New England Laminate Co (NELCO) and Polyclad in NH. Earl Moon

REWORK PROCEDURES FOR SOLDER BALLS ON BGA PKGS

Electronics Forum | Wed Feb 17 16:39:05 EST 1999 | 3D

What are some suggested standards/speced requirements and procedures for removal/addition of missing balls on laminate and ceramic based bga packages and quality requirements for same.

Reflow soldering a Flexi-Rigid pcb

Electronics Forum | Wed Apr 01 04:34:41 EST 1998 | Alan Pestell

We are looking at reflow soldering some Flexi-rigid pcbs. I have heard that IR reflow soldering can make the Polyimide "self heat" and cause de-lamination. Does anyone have any info.

Re: MLB PCB DIMENISIONAL STABILITY AND LAMINATE INTEGRITY

Electronics Forum | Tue Mar 03 13:04:36 EST 1998 | tom lambert, component engineer

We have been told that we should bakeout FR4 boards prior to assesmbly - i gather from your discussion that you disagree - any details will be sincerely appreciated. Regards.

Comparative Tracking Index (CTI)

Electronics Forum | Wed Aug 15 16:14:22 EDT 2001 | davef

Comparative Tracking Index [CTI]. In printed circuit board fabrication, CTI is a measure of the ability of the laminate surface to withstand tracking [carbonneous tracks on the surface, under wet contaminated conditions] across two electrodes placed


laminates searches for Companies, Equipment, Machines, Suppliers & Information

Circuit Board, PCB Assembly & electronics manufacturing service provider

Component Placement 101 Training Course
Solder Paste Dispensing

Stencil Printing 101 Training Course


Best Reflow Oven
Sell Your Used SMT & Test Equipment

Training online, at your facility, or at one of our worldwide training centers"
Hot selling SMT spare parts and professional SMT machine solutions

Low-cost, self-paced, online training on electronics manufacturing fundamentals