Electronics Forum | Thu Oct 08 14:04:04 EDT 1998 | Kris Ewen
Manish, I've seen similar phenomenon when processing CSPs on our cards. In our case, we were placing the components over the opening to in-pad blind vias. Due to poor drilling and plating processes by our board suppliers, volatiles were outgassing
Electronics Forum | Tue Aug 11 07:17:18 EDT 1998 | smd
Our Electrovert UPK445 needs a new solder pump motor. The Machine is down. I'm taking a huge chance with Specnor. If the motor doesn't come in or if it doesn't work, then I'm dead. They told me I'd have the motor next day. They kept trying to sell me
Electronics Forum | Tue Aug 11 12:48:09 EDT 1998 | smd
Everything went smoothly. I had the motor in less than one day. And I saved $690 from Electrovert's $1170 price (slightly different model but it works great!). | Our Electrovert UPK445 needs a new solder pump motor. The Machine is down. I'm taking a
Electronics Forum | Thu Jun 18 13:56:39 EDT 1998 | No Friend Of Alpha
So my salesman says to me that we could return our unneeded Al frames from our MPM printer to Alphametals in CA for credit to be applied toward a future sale. Sonded good. So I boxed up all the damn frames (44) and shipped them off to Goofyland. Now
Electronics Forum | Thu Aug 13 21:58:14 EDT 1998 | Alpha Guy
When things go wrong (see below) it can usually be attributed to a communication problem. This is exactly the issue with this case. A meeting has been held and corrections have been made with no hard feelings. However, another call rather than a
Electronics Forum | Sat Jun 13 07:08:46 EDT 1998 | Dave F
| Is their an IPC standard for the water that is being used in the water wash. I have been looking and at this time have not found any thing. Steve: A lot of the old command and control specification environment has changed with the "industrializati
Electronics Forum | Thu May 28 09:30:42 EDT 1998 | Chrys
| I have a component that is glue cured on the bottom of a pcb. The component is a 1206 size jumper. It is made up of iron/nickel alloy. The problem I am having is that the part will fall off the board during wave solder. Is the component not abl
Electronics Forum | Mon May 18 13:30:15 EDT 1998 | Earl Moon
| I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered and solde
Electronics Forum | Fri May 15 14:41:25 EDT 1998 | Terry Burnette 512-933-5783
| We had some failures on an IC package that the manufacturer has put down to moisture inside the package, leading to popcorning. | This seems a bit odd, the package is a PLCC 84 which is quite thick. I have only seen this problem on thin packages. |
Electronics Forum | Fri May 15 10:11:19 EDT 1998 | Justin Medernach
| We had some failures on an IC package that the manufacturer has put down to moisture inside the package, leading to popcorning. | This seems a bit odd, the package is a PLCC 84 which is quite thick. I have only seen this problem on thin packages. |