Electronics Forum | Thu Feb 12 10:19:46 EST 2004 | Bryan
Hi all, These days our customer asks us to figure out ,during reflow,the BGA ball and solder paste,which will first melt? I think it's very hard to get the rusult.coz I think it'll vary at diffrent part of the BGA,and how can this affect the perf
Electronics Forum | Fri Feb 13 11:46:23 EST 2004 | Jack
Is your customer trying to reduce voiding? If the device is using Sn90 / Pb10 and the paste is Sn63/Pb37 the board will melt first. However, if both solders are 183C eutectic, it's a tossup? PCB design, copper weight, bga type (pbga, micro bga, Tbg
Electronics Forum | Fri Oct 18 12:40:35 EDT 2013 | robertwillis
Back in the mists of time there were two papers on the use of Parylene Coating and the improved thermal cycling results in 1990. It was on LCCC then shortly after on BGA. Does anyone know of results of recent trials or have a copy of the BGA papers.
Electronics Forum | Tue Mar 14 21:09:20 EST 2000 | Dave F
Emmanuel: Take Jax's word. NiAu (ENIG) primary (some would say only) redeeming characteristic is its flatness that you mentioned, but that flatness appeals to folk placing fine pitch devices, rather than BGA. Good luck. Dave F
Electronics Forum | Tue Mar 14 21:09:20 EST 2000 | Dave F
Emmanuel: Take Jax's word. NiAu (ENIG) primary (some would say only) redeeming characteristic is its flatness that you mentioned, but that flatness appeals to folk placing fine pitch devices, rather than BGA. Good luck. Dave F
Electronics Forum | Tue Feb 17 18:17:28 EST 1998 | John Wilson
I am looking for any information or testing data done on the amount of weight that can be held by a bga package based on size of the solder sphere and number of spheres. I am reflowing components with a bga package on the opposite side and looking f
Electronics Forum | Fri Jul 12 14:35:03 EDT 2002 | jax
BGA Clamp...... Sounds to technical to me! Not sure about what is needed for installing on IP2, although I am pretty sure it can be done. I have no pic to give. Stop working with FUJI about 5 years ago.
Electronics Forum | Tue Jul 06 19:45:03 EDT 2004 | ANDREW
Based on the attchment it looks like both are low profile and cater for high IO point.What are the challenges in running this 2 type of component?Is there any additional process required other than normal SMT for these 2 packages,like underfill ?
Electronics Forum | Wed Dec 22 08:49:55 EST 2004 | markhoch
I'm looking for some data to support my argument that HASL boards are not the most ideal boards for manufacturing involving BGA's and 0402's. I'm sure one of you SMT Gurus out there can point me in the right direction! Thank you in advance!