Re: Tin-Lead thickness on PWB's/Let's Hear More

Electronics Forum | Wed May 27 11:19:34 EDT 1998 | Earl Moon

| | | | | | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered

Re: Bottom side bridging

Electronics Forum | Wed Apr 15 14:57:20 EDT 1998 | D. Lange

| | | | We are having a bridging problem with SOIC 14,16 and 20 pin devices during flow solder of the bottom side of our boards. This bridging occurs about half way up the lead between the board and the body of the IC. The chip parts are no proble

Re: Bottom side bridging

Electronics Forum | Wed Apr 15 15:04:18 EDT 1998 | D. Lange

| | | | We are having a bridging problem with SOIC 14,16 and 20 pin devices during flow solder of the bottom side of our boards. This bridging occurs about half way up the lead between the board and the body of the IC. The chip parts are no proble

Re: Bottom side bridging

Electronics Forum | Wed Apr 15 14:53:06 EDT 1998 | D. Lange

| | | | We are having a bridging problem with SOIC 14,16 and 20 pin devices during flow solder of the bottom side of our boards. This bridging occurs about half way up the lead between the board and the body of the IC. The chip parts are no proble

Re: Oven Temperature for Solder Reflow

Electronics Forum | Sun Aug 08 20:59:55 EDT 1999 | Dreamsniper

| | | What oven temperature should be used to reflow solder (Sn63Pb37) on a PC board (0.075" to 0.100" thickness) in 5 to 10 minutes? | | | | Profiling - tedious but important. As said, start with the paste manufacturers recomendation which is usua

OSP vs HASL

Electronics Forum | Mon May 14 17:12:20 EDT 2001 | davef

Continuing along the path that Brian took ... IPC-7525 gives design guideline for stepped stencils. It goes something like: * Stepped area SB GT 25 thou from pads located on the greatest thickness of the stencil * Pads in stepped area SB GT 35 tho

Foam fluxer maintenance, storage and cleaning

Electronics Forum | Mon Nov 09 09:44:22 EST 2015 | davef

Purpose. This describes setting-up a wave soldering system set-up for a new assembly design or checking a wave solder machine operation with a test board. Applicability. To be used for new design printed circuit assembles and during machine accept

Re: solder mask

Electronics Forum | Fri Aug 13 10:39:25 EDT 1999 | Boca

| | | | | | (snip) | | | | | | | | You're quite right. However, anyone who uses MeCl in an aerosol spray needs his head examining. I'll go further: if he continues, he will most CERTAINLY need his head, the rest of his CNS and his liver examining a

Re: solder mask

Electronics Forum | Thu Aug 12 22:23:23 EDT 1999 | Dave F

| | | | (snip) | | | | | | You're quite right. However, anyone who uses MeCl in an aerosol spray needs his head examining. I'll go further: if he continues, he will most CERTAINLY need his head, the rest of his CNS and his liver examining a little

Re: BGA Repair Problems

Electronics Forum | Mon Aug 17 02:50:44 EDT 1998 | Bob Willis

| Have an SRT w/preheat, 18 layer board all copper, 456 BGA needs to be removed and replaced. The manufacturer is Chip Express and during reflow it warps up or down. Causing either opens or shorts on the corners. I was using gel flux with multiple

Previous 4 5 6 7 8 9 10  

contaminated leads that cause poor wetting searches for Companies, Equipment, Machines, Suppliers & Information

PCB Handling Machine with CE

High Resolution Fast Speed Industrial Cameras.
Electronics Equipment Consignment

High Throughput Reflow Oven
SMT feeders

World's Best Reflow Oven Customizable for Unique Applications
Global manufacturing solutions provider

Nozzles, Feeders, Spare Parts - Siemens, Fuji, Juki, Yamaha, etc...


Internet marketing services for manufacturing companies