Electronics Forum | Mon Mar 29 19:17:47 EST 1999 | Scott McKee
How true, AR would not be the right choice... Scott | Just for the record folks, | | The customer I believe may be manufacturing stuff for refuelling rigs of various forms. | | This being the case, the coating would need to be resistant against f
Electronics Forum | Wed Mar 02 07:47:57 EST 2016 | deanm
Sounds like over molding would be ideal, but if they don't want to spend for a mold I would look at silicone conformal coatings that can be used in a dip process. Silicones are thicker than other coating materials and multiple drippings may provide t
Electronics Forum | Wed Jan 31 10:56:23 EST 2018 | dontfeedphils
I'm working on bringing up a new conformal coat process/workcenter and have a few questions I'm hoping someone might have experience with. Right now we're manually spraying both coating materials (1B31 and 1A33 from Humiseal) using HVLP guns. I run
Electronics Forum | Mon Jan 29 20:25:54 EST 2001 | davef
I know you're talking Humiseal, but this may help http://www.loctite.com/electronics/elec_tech_index.html Conformal Coatings (PDF Documents) "Conformal Coating Overview" (Lester D. Bennington, Senior Development Chemist and David Crossan, Manager
Electronics Forum | Tue Sep 26 08:41:27 EDT 2000 | greg
I am processing PCB's that have an n-tech osp coating and am finding huge inconsistencies in wetting. Some boards process clean with good wetting and the next has terrible wetting. The boards are stored and handled properly. Has anyone had this
Electronics Forum | Wed Sep 19 12:27:52 EDT 2012 | tombstonesmt
Looking into possibly receiving samples of polyester masking dots for conformal coating. Our usage of polymide dots have really increased in the past months and we're always looking for a reduction in costs. The only information I've found is that po
Electronics Forum | Mon Apr 17 10:21:21 EDT 2017 | dontfeedphils
So I'm starting up a conformal coating process from scratch (again, although it's been about 10 years) and I'm looking for the best option for verifying thickness. I plan on going the "coupon per setup" route which will encompass both our manual spr
Electronics Forum | Thu Oct 06 08:30:32 EDT 2005 | jdumont
What is the best/most economical way to check the thickness of conformal coating after being processed. Would a standard height gage do? Thanks in advance...
Electronics Forum | Wed May 09 03:13:06 EDT 2012 | umar
I had send my coating board to the test lab for adhesion coating test. 3 times send, the result 3times fail. The coating chemical use is Humiseal 1B31. The process is clean the boards at washing process use the Vigon A200 saponifier mix with DI wate
Electronics Forum | Fri Aug 20 12:18:11 EDT 1999 | Earl Moon
| I am being asked, by my vendor and Purchasing people about converting from Tin/lead pads on P.C.B's to Electroless Tin Plating. | Can any one tell me what I have to change in my SMT | process (paste, reflow, etc) If any? | I ran one P.C.Boar