Electronics Forum | Sun Dec 31 07:31:40 EST 2006 | davef
Thoughts are: * Eliminate solder spotting on gold fingers through process improvement in broard handling, printing paste control, and reflow recipe development. Search the fine SMTnet Archives for previous discussions. * Dispense or print a reflow te
Electronics Forum | Fri Dec 03 18:04:52 EST 2021 | SMTA-64387687
Why don't you use peelable/washable solder mask on the SMT components next to the T/H pins? Then, you won't have to worry about keeping the tight tolerances.
Electronics Forum | Sat Apr 04 15:38:10 EST 1998 | Sam Forman, MicroCoat Technologies
| I will be starting a conformal coating process soon, I am looking for any pointers on | 1) Best method for masking components, tape mask, liqued mask | 2) Which is best Spray or Dip? | 3) Compatiblity with no clean solder paste (flux residue) |
Electronics Forum | Tue Feb 19 11:08:22 EST 2002 | Chris Anglin
Guideline for Tenting Interstitial BGA Vias It is difficult to give a complete recommendation on via tenting without an idea what process conditions are required (ex: wave pass, double reflow, rework etc.). Via Pads (as Test Points) - On Bottom
Electronics Forum | Fri Feb 22 18:36:36 EST 2013 | austinpeterman
Has anyone experienced bridging on topside (solder destination side) surface mount devices after wave soldering? We x-rayed 100% of the placements after smt re-flow with no issues. When the same placements were x-rayed after the tht wave solder pro
Electronics Forum | Tue Jul 19 08:26:46 EDT 2016 | pavel_murtishev
Aleksander, The answer is no. Solder deposit being printed is 80um-150um in height depending on PCB design what is two times higher than any track covered by solder mask. Molten solder will merely center the component. QFNs are prone to soldering
Electronics Forum | Thu Aug 01 11:43:57 EDT 2019 | slthomas
I noticed that your solder mask registration is off some. Does it cover a significant portion of any of the pads for these parts? If so, is it possible that the surface tension of the solder at liquidus is enough to skew the part when the solder i
Electronics Forum | Thu May 07 13:22:37 EDT 1998 | Chrys
| I am running a board that is .062" thick and has components that over hang the edge of the board by .090". I have bottom side smt components (chip caps and resistors only) and use the turbulent wave to help solder the components. The problem I am
Electronics Forum | Thu Jul 25 21:49:55 EDT 2002 | davef
Consider: * Quitting the coating business all together and using a coating service supplier, like: Thermospray Co 800-952-5838 Mike Moninger; Advanced Coating 800-722-1444; Epsco 108 W. 37th St Boise Idaho 83714 (208)389-2000 * Buying a programmable
Electronics Forum | Fri Mar 04 11:00:37 EST 2005 | mrduckmann2000
Anybody have any ideas on the proper way to screen solder mask onto a PCB? I am going to cover SMT parts that were soldered to the btm side of the PCB, now I have to mask them in order to run this animal through the wave solder process. I know it w