Solder webbing @ Wavesolder

Electronics Forum | Tue Feb 06 13:02:36 EST 2001 | kmorris

Hi all: We are seeing "solder webbing" on the bottom side of some of our PCBs after wave solder. The solder is sticking (like a spider web) to the solder mask on the PCB. This is only happening on 2 of the many PCBs we wave on that machine. Both o

Quad Laurier Die Feeder?

Electronics Forum | Wed Feb 07 21:45:06 EST 2001 | davef

Since, 1996, Samsung has been the sole supplier of Quad component feeders. And I believe Samsung is the developer and producer of Quad�s Meridian placement machines. Quad has been fighting with Samsung for over a year [http://www.quad-sys.com/inves

Substrate Au/Ni thickness

Electronics Forum | Mon Feb 19 18:57:49 EST 2001 | davef

Expanding on the limit of the portion of gold acceptable in a solder connection [mentioned in an earlier post]: The embrittlement culprit, AuSn4, is 29 weight percent gold. So even if one had 100% tin as the solder alloy and 10% gold were dissolved

Share info for Six sigma - BB

Electronics Forum | Mon Mar 05 18:56:47 EST 2001 | davef

Stefan: Thanks for the clarification on the Siemens machine operation. Yes Stefan, Germany and some other countries have wonderful apprentice programs. Generally, we Americans have the patience of a staving gerbil for such things. Is the ON butto

Pallet Maintenance

Electronics Forum | Tue Mar 13 13:15:59 EST 2001 | kerryn

Dear Dave and Mike, I do not normally respond to threads of the forum. However, I do enjoy reading other's comments. There is a lot of valuable information provided by both suppliers and users. You seem to be making light of Bill Schreiber's com

White powdery residue following Wave

Electronics Forum | Mon Mar 05 20:53:32 EST 2001 | davef

When you say all over the board, please give more detail. Where are they located? [All over wave soldered portion, laminate only, solder mask only, solder only, specific components only, etc] When you say white residue, what color are they really?

Wavesoldering

Electronics Forum | Tue Mar 13 20:25:39 EST 2001 | davef

So, what is not soldering? Pads er test points? I assume the holes are unsupported, right? Tell us more about the test points. Are they the kind with the little pastic shoulders [on the primary side] that keep them from falling through the hole?

Gold Contacts

Electronics Forum | Wed Mar 21 16:32:03 EST 2001 | mparker

The root cause is dependant on the type of solder "splash", ball, whatever, that you are seeing post reflow. If it is smears, then cleaning the stencil underside is probably the answer. Are you using automatic wipers? How many print cycles between w

Insufficient Heel Fillets on plastic 240 pin QFPs

Electronics Forum | Wed Mar 21 20:40:28 EST 2001 | dblsixes

We are building a monster ... Dimensions are 10" x 7" ... 12 layers ... A Logic Assembly with a Power Supply all rolled into one ... The Power Supply is in one section of the board, the logic in the other section ... The Power Supply obviously has a

Insufficient Heel Fillets on plastic 240 pin QFPs

Electronics Forum | Tue Mar 27 09:06:10 EST 2001 | dblsixes

We have tried to adjust the upper and lower heaters. We have a dillema in this area however. The power supply portion of the assembly has thermal vias in the solder pads underneath larger pads. We have a problem with solder wicking through these h


problem searches for Companies, Equipment, Machines, Suppliers & Information

PCB Handling with CE

Software for SMT placement & AOI - Free Download.
Void Free Reflow Soldering

Training online, at your facility, or at one of our worldwide training centers"
pressure curing ovens

Easily dispense fine pitch components with ±25µm positioning accuracy.
Pillarhouse USA for handload Selective Soldering Needs

Have you found a solution to REDUCE DISPENSE REWORK? Your answer is here.
Electronic Solutions R3

Thermal Transfer Materials.