Dear all, we are using the lead-free SN100C solder alloy ... - Jul 13, 2007 by Dboudreau
There are a lot of areas that could be leading to this probl... - Jul 13, 2007 by jdumont
As in more dwell? We see the same problem with through ho... - Jul 13, 2007 by James
We've experienced this issue with SN100. A couple of thin... - Jul 13, 2007 by robgd3
I have zero experience with SN100c, but hey, how much diffe... - Jul 16, 2007 by Dirk Nuendyke
We haven't used no-lead yet so I can't speak to the specific... - Jul 17, 2007 by Steve Thomas
You want to know which flux will over come thermal mass prob... - Jul 17, 2007 by Hussman
SOOOO true!!! ... - Jul 19, 2007 by aisart
Well, everyone has provided good advice, but if you are look... - Jul 31, 2007 by Rafael