We are looking into switching SMT adhesives, because of the ... - Jul 17, 2007 by Dback
Hey DBack! The 80's called. They want their pump dispensin... - Jul 17, 2007 by Dirk Nuendyke
Actually, you just decribed what I am wearing, down to the h... - Jul 17, 2007 by Dback
It has been my experience that Loctite is the best. Call th... - Jul 17, 2007 by Sr. Tech
We use Loctite 3609 chipbonder. Works well for us. ... - Jul 17, 2007 by SWAG
Yuppers. Back in the "late '90s" at my last company, we, to... - Jul 17, 2007 by Dirk Nuendyke
We've used the Loctite as well. We're currently using Her... - Jul 17, 2007 by John S.
Thank you all for your suggestions, I will get samples of th... - Jul 17, 2007 by Dback
They still make SMT adhesive?!?!?! Holy SMOKES BATMAN. I ... - Jul 18, 2007 by Ed Faranda
Loctite 3609 is a pretty good smt adhesive. I'd actually rec... - Jul 19, 2007 by bruce
Wait...stop! Some adhesives will void when cured... some co... - Jul 19, 2007 by D Wanzek
Wow, I've never heard of this. If it voids during cure you ... - Jul 20, 2007 by Hussman
SMT adhesive is hydroscopic. Some types absorb moisture fas... - Jul 20, 2007 by Sr. Tech
Guess I've been spoiled using Loctite brands for the past 20... - Jul 20, 2007 by Hussman
Good luck. Loctite will work just fine if other combination... - Jul 20, 2007 by D Wanzek
What? D Wanzek works for Heraus?!?!? Jeez, these f*cking s... - Jul 20, 2007 by Hussman
Hi Huss, Didn't you notice the names, "D Back" and "D Wan... - Jul 20, 2007 by Real Chunks
Hey Real Chunks, my question was legit, don't use my name to... - Jul 24, 2007 by Dback
:^( Sorry. ... - Jul 24, 2007 by Real Chunks
I have been using the Heraus paste for almost ten years. At ... - Jul 24, 2007 by adlsmt
since 1999 we use Heraeus PD944, in time we tested Loctite a... - Jul 26, 2007 by d0min0
Hope you found an adhesive that works for you Dback. Thou... - Sep 05, 2007 by D Wanzek
So that's why you open old wounds? ... - Sep 05, 2007 by Real Chunks