Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 5023
Something unusual happened yesterday, we reflow soldered two...
- Mar 04, 2006
by
JimD
Epoxy inks tend to be more resistant to discoloration than t...
- Mar 06, 2006
by
davef
I have had the purple silkscreen, I don't remember the exac...
- Mar 06, 2006
by
RDR
Thanks Russ. As it turned out, it was an incomplete cure at ...
- Mar 12, 2006
by
JimD
We had the same issue on a batch of boards and the board hou...
- Mar 12, 2006
by
Our PCB also had this process.
...
- Mar 13, 2006
by
RDR