beryllium copper

Views: 2440

#40405

beryllium copper | 14 March, 2006

Q: Is anyone aware of any solderability issues that may exist when soldering beryllium copper parts (in this case spring contacts) to a PCB using standard Pb63/Sn37 solder paste/wire?

reply »

#40414

beryllium copper | 14 March, 2006

BeCu is not solderable without plating Cu, Sn, Ag, Ni etc. The solder joint will only be as strong as the bond strength of the solderable plating to the BeCu