Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 4322
Hi, i tried to search but am hving trouble finding discuss... - Apr 07, 2006 by Raquel
Technically speaking, most likely yes it will work, unless p... - Apr 07, 2006 by muse
Is it safe to assume that you're only talking about SMT refl... - Apr 07, 2006 by Steve Thomas
Yes, sorry, I have no detailed experience with wave-solderin... - Apr 07, 2006 by muse
Thank you! sorry, i just realized my posted question was not... - Apr 13, 2006 by Raquel
yep, only SMT reflow. ... - Apr 13, 2006 by Raquel
If your part will withstand the higher pbfree reflow temp yo... - Apr 13, 2006 by RDR
Hi russ, I am in the process of developing a "hybrid" reflo... - Apr 14, 2006 by Amol Kane
thanks! yes, the package has been qualified using 260deg max... - Apr 20, 2006 by Raquel
yes! i though this thread looked familiar! looks like it has... - Apr 21, 2006 by Amol Kane