Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 2886
Hello All, Could someone offer suggestions to cure poor B... - Apr 18, 2006 by
Don't comprehend the baseball cap comparison, could you try ... - Apr 18, 2006 by RDR
Sorry about that. I'd like to post a picture but doubt it's ... - Apr 19, 2006 by
So, your solder ball didn't collapse. What is the ball mate... - Apr 19, 2006 by davef
That would be correct. Some others call it `Head in Pillow'.... - Apr 26, 2006 by
So does the defect follow the part or the orientation of the... - Apr 26, 2006 by RDR
Hi Russ, The board was ran in two orientations but with p... - Apr 26, 2006 by
Carol Stirling