Hi,
Can anyone recommend a leadfree recipe for a BTU VIP9...
- May 24, 2006
by
GEB
how many zones?
And what settings are you using now?
And...
- May 24, 2006
by
Stephen
Do you really need to have that shape of profile, why not ha...
- May 24, 2006
by
7 zones.
AIM solder SAC305.
...
- May 24, 2006
by
GEB
VIP 98, I believe that's a 7 zone if I can remember 6 years ...
- May 24, 2006
by
GEB,
Datasheets are usually just guidelines and most App. E...
- May 24, 2006
by
Samir Nagheenanajar
I have 4 of these furnaces.
Give me your length, width, m...
- May 24, 2006
by
Thank you - The PCB weighs 192.9g and is 314mm x 228mm. Not ...
- May 26, 2006
by
GEB
Cheers Samir, that was a great help! I've tweaked the settin...
- May 26, 2006
by
GEB