Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 5626
Why do they say to specify the depth of the score, rather th... - Jun 12, 2006 by muse
As far as wich is spec'd it makes no diiference since they h... - Jun 12, 2006 by RDR
IPC spec is V-score shall not be more than 1/2 board thickne... - Jun 12, 2006 by PeteC
Which spec is that in? I'm seeing web thicknesses of .015 o... - Jun 12, 2006 by muse
Its in the IPC 600 bare-board specification. ... - Jun 12, 2006 by PeteC
Hi, A little off subject but I just finished a quick litt... - Jun 12, 2006 by Flipit
OK, Pete, I just looked all through IPC-A-600G. Saw no ment... - Jun 12, 2006 by muse
IPC-2222, 5.3.1 defines the parameters of making scoring cut... - Jun 13, 2006 by davef
Hi all, The majority of score machines used today have a ... - Jun 14, 2006 by