Hi All,
We have a board that's going through our proce...
- Jun 19, 2006
by
Try to dip that wire with flux before insert to PCB. IT's wi...
- Jun 19, 2006
by
So, a 10SWG is about an 8AWG.
We can't think of a IPC sta...
- Jun 19, 2006
by
davef
I, too, would bend it 90-degrees prior to assembly and I wou...
- Jun 20, 2006
by
FD
What is your process? Wave solder, hand solder, pin in past...
- Jun 20, 2006
by
It's hand solder, the wires are free issued, what i'm findin...
- Jun 20, 2006
by
I was afraid so. Hand soldering wires in general is not dif...
- Jun 20, 2006
by
The minimum vertical hole fill is defined as follows:
Class...
- Jun 20, 2006
by
davef
Agreed! More soldering irons will provide the solder joint ...
- Jun 21, 2006
by
Dr Shocker
You may want to pre tin wires then dip into flux before sold...
- Jun 21, 2006
by
RDR
dougs