Hi all, I wonder if some of you have experience in use of dr...
- Jul 31, 2006
by
We use 5744 with good results. It remains solid (granular) a...
- Aug 01, 2006
by
Steve Thomas
Be careful and review the MSDS sheets on any dross inhibitor...
- Aug 02, 2006
by
Steve
What is the name of the dross eliminator you are referring t...
- Aug 07, 2006
by
I would be interested to see what Dross eliminators are avai...
- Aug 08, 2006
by
You can find some interesting stuff regarding MS2 here in th...
- Aug 08, 2006
by
Steve Thomas
Hello all, just wanted to say that I've been using MS2 for 2...
- Aug 08, 2006
by
John,
What is the cost/litre?
aj...
...
- Aug 09, 2006
by
I paid $168/ liter for the leaded on my recent order of 24 l...
- Aug 10, 2006
by
John,
What about the machine? I understand that pumps nee...
- Aug 11, 2006
by
You can contact Graphic Research and Brad Koor will tell you...
- Aug 14, 2006
by
Baer
We've just conducted an MS2 study, and we found very little ...
- Aug 14, 2006
by
Hello everybody, My name is Jay Hardin and I'm the MS2 Appli...
- Aug 17, 2006
by
hi aj, I am interested to know where do you get the solder s...
- Aug 21, 2006
by
Pulsar Solder Saver: "The Solder Saver is a unique, handheld...
- Aug 21, 2006
by
davef
I have just finished a trial on the "Pulsar Solder saver Uni...
- Aug 22, 2006
by
Dear Sir,
We produce solder dross reducing Powder and wave ...
- Sep 04, 2006
by
Just reading these comments are really interesting but very ...
- Sep 07, 2006
by
Greg, can you share what is this metallic anti drossing agen...
- Sep 25, 2006
by
Sorry Bert
For some reason I'm not getting the Email noti...
- Oct 04, 2006
by
Betsy