We are looking to possibly counterbore a coule of thru holes... - Aug 17, 2006 by markb
It sounds more expensive just at face value than better LEDs... - Aug 17, 2006 by Steve Thomas
Well, you won't win any IPC awards for doing this. Another ... - Aug 17, 2006 by
Steve - The weakened condition was my concern, and that was ... - Aug 17, 2006 by markb
I don't have any data (haven't tried this), but it doesn't t... - Aug 17, 2006 by Steve Thomas
We use plastic standoffs that fit between the LED and the bo... - Aug 17, 2006 by davef
Thank for the feedback everyone. The LED is designed to b... - Aug 18, 2006 by markb
Steve, You almost got yout Man Card revoked for stating: ... - Aug 18, 2006 by
Hi Mark, Couterbore is possible in two way's during PCB M... - Aug 18, 2006 by
blasted double post ... - Aug 18, 2006 by Steve Thomas
Not sneakin' anything past you, are we Chunks? :P ... - Aug 18, 2006 by Steve Thomas
Does that make me a "Master" of post reading? ... - Aug 18, 2006 by