All, We have a conveyor that uses an o-ring belt , this b... - Aug 21, 2006 by
You can try Larrying .... I mean BUTTing them together and u... - Aug 21, 2006 by
....or a soldering iron ... - Aug 21, 2006 by Rob
Chunks, I figured you would know about O rings. :/ Try ... - Aug 23, 2006 by Sr. Tech
I think cyanoacrylate is the glue of choice for buna-n, but ... - Aug 23, 2006 by Steve Thomas
At a previous job we had a kit to splice the belts. It was ... - Aug 23, 2006 by jdengler
Super glue too. It's not just for sniffing anymore... Do... - Aug 23, 2006 by
Hi Jerry- The belt splice kit we used were made by Eagle Be... - Aug 24, 2006 by nodlac
Hi, this is not a solution for your o-ring "belt" problem bu... - Aug 26, 2006 by