We are having intermittent faults with BGA's soldered onto a...
- Nov 13, 2006
by
saaitk
Good afternoon,
1. Never heard that phosphorus crystals f...
- Nov 13, 2006
by
Hypnotia
do you mean too much gold brightener that dewetts solder???
...
- Nov 13, 2006
by
You said your gold processing is immersion. More importantl...
- Nov 13, 2006
by
davef
Thanks for your input folks. I will have to get back to our ...
- Nov 14, 2006
by
saaitk
Good afternoon,
Yes, it is to be expected. This is well k...
- Nov 14, 2006
by
Hypnotia