i have 1 customer using our reflow oven, he is facing the pr... - Jan 06, 2007 by india123
Hi. How one Can suggest you unless your Involment in your... - Jan 06, 2007 by shrikant_borkar
There may be a coating on the components that fell-off that ... - Jan 06, 2007 by davef
I had the same problem. However, now that I switched to cra... - Jan 07, 2007 by
Some IC's have their body away from the board. Is the glue ... - Jan 08, 2007 by Stephen
With us, it was the component coating! try other make or ve... - Jan 18, 2007 by Peter, Belgium
kindly send me your reflow profile ---and also the PCB lay o... - Jan 19, 2007 by
I have seen this before. Check: --Vibration of belt --In... - Feb 07, 2007 by