I am soldering a Germanium Window with a metalized rim to a ... - Jan 09, 2007 by Brian E
Brian, There are a couple of ideas that you can use for t... - Jan 10, 2007 by Mario Scalzo - CSMTPE, Dartmouth 6 Sigma Brown Belt
> I am soldering a Germanium Window with a > metaliz... - Jan 10, 2007 by Flipit
Thanks both of you for responding. I am using a protoype re... - Jan 11, 2007 by Brian E
Mario, I tried a couple of profiles. In all cases the pr... - Jan 11, 2007 by Brian E
The N2 would allow you to use less flux since the oxidation ... - Jan 11, 2007 by Flipit
it's a vacuum dewar so adhesives will eventually permeate an... - Jan 11, 2007 by Brian E