Hello, we are facing some troubles with BGA opens in our... - Jan 24, 2007 by Frank
Tricky stuff. I would expect to hit between 210-215 peak ... - Jan 25, 2007 by
Thank you for feedback and comment. We are trying this a... - Jan 30, 2007 by Frank
these assemblies getting depaneled? ICT? any fixtures or any... - Jan 30, 2007 by RDR
Profile should have a longer cool soak. Verify as was ment... - Feb 04, 2007 by
...and, bake those parts. A lot of times, moisture will caus... - Feb 07, 2007 by BillyD
FRank, are the BGA's in question a no-lead part? This usual... - Feb 20, 2007 by ehess
Dear SMT community, thank you all for your comments and ... - Feb 25, 2007 by Frank
Just make sure you keep the half done assemblies in dry stor... - Feb 25, 2007 by Stephen