The QFN is found to have contact problem during FCT. The pas... - Feb 06, 2007 by
Water soluble residues probably won't cause instant failures... - Feb 07, 2007 by JAX
Had the very same thing happen the first time we used the sm... - Feb 07, 2007 by BillyD
Wayne