I know this subject has been beat to death, but I need a cla...
- Feb 07, 2001
by
Steve T.
You're correct that some folk have used microns and other fo...
- Feb 07, 2001
by
davef
The ENIG process will yield between 3-7 micro inches (110 - ...
- Feb 09, 2001
by
Doug Benefiel
Yes this does help. Thanks for your input.
...
- Feb 12, 2001
by
Steve T.
u" are smaller. 1uM = 39.4u" and so 3-7uM = 118-275u"
Th...
- Feb 21, 2001
by
Dave E
Steve T.