Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
We are reviewing our shelf life policy and have the followin...
- Feb 07, 2001
by
davef
-Surface mount adhesives (any other adhesives)
-Roll sol...
- Feb 08, 2001
by
K
K: Do you shelf life control rolled solder because of the f...
- Feb 08, 2001
by
davef
Nope -- we don't shelf life control roll solder here.
Just ...
- Feb 08, 2001
by
K
Any adhesive tape, or stuff that uses it in packaging, like ...
- Feb 08, 2001
by
Steve Thomas
Potting compounds and conformal coatings.
Any 1 or 2 com...
- Feb 08, 2001
by
We maintain shelf life on all of our RTV silicon compounds.
...
- Feb 13, 2001
by
We got dinged in a ISO 9000 audit for not having shelf life ...
- Feb 13, 2001
by
LarryK
From Kester's web site:
"Flux cored solder wire has a lim...
- Feb 14, 2001
by
Steve Thomas