I have done some simple DOE and found that substrate with
t...
- Feb 15, 2001
by
What do you mean by "But after performing temperature cycle ...
- Feb 15, 2001
by
davef
Expanding on the limit of the portion of gold acceptable in ...
- Feb 19, 2001
by
davef
Thanks Dave for your helpful response.
I found that the thi...
- Feb 20, 2001
by
Let�s be basic. The two most common causes of BGA opens tha...
- Feb 20, 2001
by
davef
Nick